Abrasion Resistant Plate

WINCO-TUF 36

Hi Strength Wear Plate. Quenched and Tempered for Extreme Abrasion and Impact.

WINCO-TUF 36 has excellent toughness at high hardness and in heavy sections. For severe impact and abrasion.

Advantages

  • Maximum resistance to abrasion and impact.
  • Withstands the brittleness which develops at subnormal temperatures.
  • Increased toughness and fatigue resistance.
  • Retains high strength and wearability at high temperatures.
  • High impact and wear properties retained at weld joints.

Physical Properties

Tensile Strength — 200,000 PSI
Yield Strength — 160,000 PSI
Elongation in 2″ — 14.4%
Reduction of Area — 55%
Hardness — 36-44 Rockwell “C”
Brinell — Min. 360

Typical Analysis

Carbon — .17/.25

Chromium — .45/.60

Manganese — 1.35/1.85

Nickel — .40/.70

Silicon — .35/.45

Copper — .60/.75

Molybdenum — .35/.45

Phosphorus — .025 max.

Sulphur — .025 max.

WINCO-TUF 40

Superior to standard AR400. Hi Strength Wear Plate. Quenched and Tempered for Extreme Abrasion and Moderate Impact

WINCO-TUF 40 has excellent toughness at high hardness and in heavy sections. For severe abrasion…and superior to standard AR400. Winco-Tuf 40 is for use in areas where AR400/AR500 are currently used.

Advantages

  • Maximum resistance to abrasion and impact.
  • Withstands the brittleness which develops at subnormal temperatures.
  • Increased toughness and fatigue resistance compared to low carbon and 1045 plate.
  • Retains high strength and wearability at high temperatures.
  • High impact and wear properties retained at weld joints.

Physical Properties

Tensile Strength — 200,000 PSI

Yield Strength — 160,000 PSI

Elongation in 2″ — 14.4%

Reduction of Area — 55%

Hardness — 40-46 Rockwell “C”

Brinell — Min. 375-440

Typical Analysis

Carbon — .17/.25

Chromium — .45/.60

Manganese — 1.50

Nickel — .70/1.00

Silicon — .50

Copper — .15/.30

Molybdenum — .20/.60

Phosphorus — .025 max.

Sulphur — .015 max.

WINCO-TUF 50

Superior to standard AR500. Ultra Hi Strength Alloy Wear Plate.

WINCO-TUF 50 Quenched and Tempered, High Alloy Steel Is Intended Specifically for Applications Requiring a High Degree of Abrasion and Wear Resistance.

Used by industries such as mining, forestry, quarrying, and construction. WINCO-TUF 50 is the cost-effective choice for parts subjected to extremely high levels of wear. Winco-Tuf 50 if superior to standard AR500 plate. Winco-Tuf 40 is for use in areas where AR400/AR500 are currently used.

Physical Properties

Tensile Strength — 210,000 PSI

Yield Strength — 180,000 PSI

Elongation in 2″ — 12%

Hardness — 48-53 Rockwell “C”

Brinell Hardness — 455-525 BHN

Typical Analysis

Carbon — .31

Chromium — 1.00

Manganese — 1.50

Nickel — .70

Silicon — .55

Boron — .003

Molybdenum — .35

Phosphorus — .025

Sulphur — .015

Welding Instructions

WINCO-TUF 50 has superior welding characteristics. No specific electrodes are needed — standard low-hydrogen, high-tensile rod is recommended for maximum strength. E100XX, E110XX or E120XX or E130XX is preferred.